机构地区:[1]浙江大学材料科学与工程学系,浙江杭州310027
出 处:《压电与声光》2010年第4期657-659,共3页Piezoelectrics & Acoustooptics
基 金:supported by the projects of national key technology support program (2009BAG12A07)~~
摘 要:研究了添加不同CuO-H3BO3含量的(Ca0.61,Nd0.26)(Ti0.98Sn0.02)O3(CNT)陶瓷的烧结行为和介电性能。研究表明:CNT陶瓷的烧结温度能降低近300℃,没有观察到第二相,完全形成了钙钛矿结构固溶体。少量CuO-H3BO3能促使陶瓷在1 050℃致密烧结而不严重破坏其介电性能。添加5wt%CuO-H3BO3的CNT陶瓷在1 050℃烧结后具有良好的微波介电性能:εr=92,Q×f=9 250 GHz,τf=+139×10-6/℃。Sintering behaviors and microwave dielectric properties of the (Ca0.61,Nd0.26)(Ti0.98Sn0.02)O3(CNT) ceramics with different amounts of CuO-H3BO3 addition had been investigated in this paper.The sintering temperature of CNT had been efficiently decreased by nearly 300 ℃.No secondary phase was observedin the CNT ceramics and the complete solid solution of the complex perovskite phase was confirmed.CNT ceramics with small amounts of CuO-H3BO3 could be well sintered at 1 050 ℃for 2 h without much degradationin the microwave dielectric properties.Especially,CNT ceramics with the 5wt.% CuO-H3BO3 sintered at 1 050 ℃ have optimum microwave dielectric properties ofεr=92,Q×f=9 250 GHz,andτf=+139×10-6/℃.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:18.117.157.50