90t钢包炉底吹氩工艺优化的水模拟试验研究  被引量:3

A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace

在线阅读下载全文

作  者:丁宁[1,2] 包燕平[1] 孙齐松[2] 王立峰[2] 

机构地区:[1]北京科技大学冶金与生态工程学院,北京100083 [2]首钢技术研究院,北京100043

出  处:《特殊钢》2010年第5期8-10,共3页Special Steel

摘  要:采用1:2.5几何相似比的水模型,试验研究了钢厂90 t钢包炉(LF)透气砖位置、数量和底吹供气量对钢包内流体混匀时间的影响。结果表明,优化后的钢包透气砖位于高位料仓下料位置的下方,渣料和合金能够直接加在裸露区,熔化速度快,合金收得率高;底吹气体流量23.89 L/min时钢包流体混匀时间最短,有利于钢水深脱硫。The effect of location and number of gas permeable brick and bottom argon supply rate on mixing time of liquid in a 90 t ladle furnace at steelworks has been tested and studied by using water model with 1 : 2.5 geometric resemble scale. Results show that the optimum ladle furnace gas permeable brick is located under dumping area of high level charging hopper, the slag material and alloy is directed adding at bare area to get higher melting rate and alloy yield; and the mixing time of liquid in ladle is shortest with bottom gas blowing rate 23. 89 L/min, it is available to deep desulphurization of liquid steel.

关 键 词:钢包炉 底吹工艺 混匀时间 水模拟 

分 类 号:TF769[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象