作 者:云娜[1,2] 陈思杰[1] 钟愉曾[1] 钟敏郡[1] 林长浓[1]
机构地区:[1]广东轻工职业技术学院,广东广州510300 [2]华南理工大学制浆造纸工程国家重点实验室,广东广州510640
出 处:《造纸科学与技术》2010年第6期29-32,共4页Paper Science & Technology
摘 要:本实验研究了废纸脱墨浆的FAS漂白工艺及其影响因素,探讨了FAS用量、NaOH用量、温度、时间对纸浆白度的影响,以及FAS漂白(F)和TAED活化H2O2(P)两段漂白工艺条件。结果表明,影响废纸脱墨浆漂白效果的顺序为:FAS用量>时间>温度>NaOH用量;废纸脱墨浆FAS漂白的最佳工艺条件为:FAS用量0.6%,NaOH用量0.3%,温度70℃,时间30min。PF两段漂白优于FP两段漂白。FAS bleaching technology and affecting factors as well as FAS(F) TAED activated H2O2(P) two stages bleaching of deinked pulp were studied in this paper.The results showed that the sequence of FAS bleaching affecting factors was FAS dosage,reaction time,temperature and NaOH dosage.The optimum bleaching conditions were FAS 0.6%,NaOH 0.3%,reaction time 30min,temperature 70℃.PF two-stage bleaching was better than FP two-stage bleaching.
关 键 词:废纸脱墨浆 FAS TEAD活化H2O2 漂白
分 类 号:TS749.7[轻工技术与工程—制浆造纸工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.249