无捕收剂浮选提高金矿回收率试验研究  

Study on the increase of gold recovery with Collectorless

在线阅读下载全文

作  者:刘建业 刘杰[2] 张淑敏[2] 崔峥[3] 

机构地区:[1]辽宁省矿产勘查院,辽宁沈阳110031 [2]东北大学资源与土木工程学院,辽宁沈阳110004 [3]沈阳计量测试院,辽宁沈阳110179

出  处:《中国科技博览》2011年第6期72-74,共3页China Science and Technology Review

摘  要:为建设环保矿山并提高金矿回峰率,进行了无捕收剂浮选的试验研究。对磨矿细度、调整剂用量、硫化钠用量、起泡剂用量等条件进行了研究。结果表明,采用无捕收剂浮选工艺,在原矿金品位16.75g/t,磨矿细度细度-0.074mm占60%、硫化钠用量600克/吨,2#油用量234.8g/t、浮选时间24min的情况下,可获得金精矿平均品位45.96g/t、回收率96.33%的技术指标。比选矿厂原生产指标(92%左右)提高了4%以上的回收率。Collectorless flotation process was studied to increase gold recovery from gold ore and construct environmental mining. Under such conditions of gold grade of run-of mine ore 16.75g/t, grinding fineness (-0. 074mm) 60%, sodium sulfide 600g/t, 2# oil 234.8 g/t and flotation time 24min, the concentrate with gold grade of 45.96g/t and recovery of 96.33% were achieved and the recovery from this paper is more 4% than the original index (92%) in the dressing plant.

关 键 词:无捕收剂 浮选 金矿 回收率 

分 类 号:TD953[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象