锅炉给水加氧处理中钝化膜性能的试验研究  被引量:9

Experimental Study of Passive Film Formed by Oxgenated Treatment of Boiler Feedwater

在线阅读下载全文

作  者:周臣[1] 钱洲亥[1] 祝郦伟[1] 肖修林[1] 于志勇[1] 冯礼奎[1] 曹求洋[1] 

机构地区:[1]浙江省电力试验研究院,杭州市310014

出  处:《电力建设》2011年第7期68-72,共5页Electric Power Construction

摘  要:介绍了锅炉给水加氧处理中钝化膜的形成机理和保护性能,并对某厂1000MW超超临界机组锅炉给水加氧停止后钝化膜的保护性能进行了一系列的试验。试验研究结果表明锅炉给水在停止加氧后,钝化膜在很长一段时间仍具有保护性。同时,对锅炉给水采用间断性加氧方式的可行性进行了探讨。The formation mechanism and protection performance are introduced of the passive film formed by oxgenated treatment of boiler feedwater.A series of experiments about the protection performance of the passive film are conducted after oxygenated treatment of boiler feedwater is ceased in 1000 MW ultra-supercritical units.It is shown that the passive film is also protective for a long period.Furthermore,it is feasible for the boiler feedwater to be discontinuously oxygenated.

关 键 词:锅炉给水 加氧处理 钝化膜 保护性能试验 间断性加氧 流动加速腐蚀 

分 类 号:TM734[电气工程—电力系统及自动化]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象