弱氧化性气氛下尘泥含碳球团的还原动力学  被引量:5

Reduction Kinetics of Carbon-containing Pellets Made of Dust and Sludge under Weak Oxidizing Atmosphere

在线阅读下载全文

作  者:魏汝飞[1] 李家新[1] 李杰民[2] 龙红明[1] 王平[1] 高岗[1] 林高鹏[2] 

机构地区:[1]安徽工业大学冶金与资源学院,安徽马鞍山243002 [2]马鞍山钢铁股份有限公司第三炼铁总厂,安徽马鞍山243000

出  处:《过程工程学报》2011年第3期429-435,共7页The Chinese Journal of Process Engineering

摘  要:在1348~1573K温度范围内,在弱氧化性气氛下还原尘泥含碳球团,通过动力学实验和还原机理分析,得出影响尘泥含碳球团还原速度的限制性环节为界面反应或局部反应,反应活化能为111.66kJ/mol,还原速度可由Mckewan方程1-(1-R)1/3=kt表达.随温度升高,反应速率增大,金属化率和脱锌率提高,金属化率和脱锌率1573K时最高,分别为79.92%和97.83%,1348K时最低,仅为60.17%和75.25%.Reduction experiment of carbon-containing pellets made of dust and sludge under weak oxidizing atmosphere in the temperature range from 1348 to 1573 K was conducted. By studying its kinetics and analyzing reduction mechanism, it is found that the restriction step of the reduction rate of pellets is interfacial reaction or local reaction, and the activation energy 111.66 kJ/mol, and the reduction rate of pellets can be expressed by Mckewan equation 1-(1-R)^1/3=kt. In addition, temperature is an important factor influencing reaction rate, dezincification and metallization rates increase with temperature rising. Dezincification and metallization rates attain the maximum 97.83% and 79.92% respectively at 1573 K, compared with the minimum 75.25% and 60.17% at 1348 K.

关 键 词:尘泥 含碳球团 还原动力学 氧化性气氛 

分 类 号:TF533.1[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象