机构地区:[1]苏州市兴业铸造材料有限公司,江苏苏州215151
出 处:《铸造》2011年第8期794-795,810,共3页Foundry
摘 要:自硬呋喃树脂砂砂型有较高的常温强度和高温刚性,金属液浇注后,铸型退让性较差,阻碍铸件收缩,产生较大应力,诱使铸件产生裂纹缺陷,尤以铸钢件为甚。为攻克自硬呋喃树脂砂高温退让性这一技术难题,从多技术方案中优选丙酮改性和特殊助剂的技术方案,取得了事半功倍的效果。The no-bake furan resin sand mold has comparatively higher room temperature strength and high temperature rigidity. After pouring liquid metal, the poor deformability of the mold impedes the contraction of castings, and generates relatively higher stress which leading to the crack defects of the castings, especially for steel castings. In order to solve the problem above, the technical scheme of acetone modification with special accessory ingredient was preferentially chosen from many schemes, and twice the results were obtained with half the effort.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.62