新型无熟料矿渣水泥的试验研究  被引量:9

Experimental Study on the New Non-clinker Slag Cement

在线阅读下载全文

作  者:张明涛[1] 赵敏[1] 谭克锋[1] 

机构地区:[1]西南科技大学材料科学与工程学院,绵阳621010

出  处:《硅酸盐通报》2011年第4期920-924,共5页Bulletin of the Chinese Ceramic Society

摘  要:以高炉矿渣为主要原料,添加Ca(OH)2、CaCO3、可溶性钙盐等辅助材料可在pH值较低的条件下制备出一种不需煅烧的无熟料水泥,该水泥中矿渣掺量可达80%,强度可达国标42.5级水泥要求。Ca(OH)2、CaCO3可以激发矿渣的活性,可溶性钙盐的加入降低了水泥的pH值,进一步激发了矿渣的活性。其主要水化产物为C-S-H凝胶和水化碳铝酸钙。The Non-clinker cement with lower pH was prepared with blast furnace slag as the main raw material, and Ca( OH)2, CaCO3, soluble calcium salts as support materials. The slag in the cement reached up to 80% and the Non-clinker cement meets the requirements for strength class 42.5. Ca(OH) 2 combined with CaCO3 stimulate the activity of slag, which was further stimulated by lowering the pH values by the addition of soluble calcium salts. The main hydration products were the carbon-calcium aluminate and C-S-H gel.

关 键 词:矿渣 无熟料水泥 PH值 

分 类 号:TQ172[化学工程—水泥工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象