AD24井φ139.7mm钻杆接头断裂分析  被引量:3

Rupture Analysis of φ139.7 mm Drill Pipe Joints in AD24 Well

在线阅读下载全文

作  者:易浩[1] 吕庆钢[1] 陈勇 刘志良 张胜鹏 雷正义[3] 

机构地区:[1]中国石化西北油田分公司工程技术研究院器材供应中心,乌鲁木齐830011 [2]西部钻探钻井工程技术研究院,新疆克拉玛依834000 [3]吉林油田公司工程技术处,吉林松原138000

出  处:《石油矿场机械》2011年第9期62-65,共4页Oil Field Equipment

摘  要:采用有限元技术分析了AD24井φ139.7 mm钻杆断裂失效的原因,利用测量统计结果得出双台肩钻杆接头承载能力大幅下降是钻杆接头产生疲劳断裂的主要原因,为采取相关的预防措施提供了理论依据。The φ139.7 mm pipes were used to drill in AD24 well,crack happened on 39 pipes.With a large proportion of rupture,it had inherent reasons.Therefore,finite element technique was adopted to quantitatively analyzing the reasons of the failure,in order to take corresponding prevention measures to provide theoretical basis.Moreover measuring statistical results were used and bearing capacity decreasing of double shoulder pipe joints was the main reason of fatigue fracture.

关 键 词:钻杆 断裂 测量统计 双台肩接头 

分 类 号:TE921.2[石油与天然气工程—石油机械设备]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象