作 者:方臻飞[1] 李丽[1] 沈向前[1] 胡信群[1] 唐建军[1] 吕晓玲[1] 唐亮[1]
机构地区:[1]中南大学湘雅二医院心内科,湖南省长沙市410011
出 处:《中国组织工程研究与临床康复》2011年第34期6296-6301,共6页Journal of Clinical Rehabilitative Tissue Engineering Research
摘 要:背景:研究表明普通镍钛合金先天性心脏病封堵器镍钛合金表面钝化膜可被破坏,在复杂的机体内环境中其内部镍离子释放使血镍增高,导致封堵器的组织相容性恶化。目的:评价新型生物陶瓷膜先天性心脏病封堵器的安全性与有效性。方法:先天性心脏病患者110例,其中房间隔缺损46例,室间隔缺损32例,动脉导管未闭32例。按手术先后顺序进行区组随机分组,两组病例各占一半,实验组置入陶瓷膜封堵器CeraTM,对照组置入普通镍钛合金封堵器HeartRTM,术后24h,1,3,6,12个月随访观察并发症的发生及心功能改变,包括临床体格检查,经胸超声心动图,心电图以及胸片结果。结果与结论:对照组1例房间隔缺损置入后20h封堵器脱落,实验组1例房间隔缺损封堵失败,其余患者均成功置入封堵器。置入两种不同封堵器患者在血流动力学资料改善,术中导管操作数据,残余分流率,并发症发生率,减少心脏超容量负荷,改善肺血增多等方面差异无显著性意义(P>0.05)。说明生物陶瓷膜先心病封堵器临床疗效及安全性与普通镍钛合金封堵器无差异。BACKGROUND:Studies have demonstrated that the nickel-titanium alloy passive film of common nitinol occluders in congenital heart disease can be destroyed,its internal nickel ion release increases the blood of nickel in complex organic internal environment,and leads to histocompatibility worse of occlude. OBJECTIVE:To evaluated the safety and effectiveness of the new CeraTM occluder. METHODS:A total of 110 cases with congenital heart disease patients,including 46 cases with atrial septal defect(ASD) ,32 cases with ventricular septal defect,and 32 cases with patent ductus arteriosus. According to the operation sequence using block randomized method,the patients were assigned to experimental group(CeraTM occluder) and control group(HeartRTM) . The incidence of complication and changes of heart function were observed at 24 hours,1,3,6 and 12 months follow-up,including clinical examination,transthoracic echocardiography,electrocardiography,and chest X-rays results. RESULTS AND CONCLUSION:The occluder of 1 case with ASD desquamated at 20 hours after implantation in control group. Except one patient of ASD in the experimental group,109 patients were successfully implanted occluders in the institution. There was no significant difference in haemodynamics data,procedural data,residual shunt rate and incidence rate of complication,the reduction of cardiac volume overload,and the improvement increased of pulmonary blood flow(P 0.05) . The biocermic coating(CeraTM) has the same clinical safety and effectives,compared with common nitinol occlude(HeartRTM).
关 键 词:生物陶瓷膜 先天性心脏病 镍钛合金 封堵器 介入治疗
分 类 号:R318[医药卫生—生物医学工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.28