还原焙烧-磁选回收氰化尾渣中铁的试验研究  被引量:21

Recovery of Iron from Gold-cyanide Residue by Reduction Roasting and Magnetic Separation

在线阅读下载全文

作  者:尚德兴[1] 陈芳芳[2] 张亦飞[2] 曾鸣[1] 

机构地区:[1]中国矿业大学(北京)化学与环境工程学院,北京100083 [2]中国科学院过程工程研究所绿色过程与工程院重点实验室,湿法冶金清洁生产技术国家工程实验室,北京100190

出  处:《矿冶工程》2011年第5期35-38,共4页Mining and Metallurgical Engineering

基  金:国家水体污染控制与治理科技重大专项项目(2009ZX07529-005)

摘  要:以褐煤为还原剂,采用还原焙烧-磁选的方法回收氰化尾渣中的铁,考查了褐煤添加量、焙烧温度、焙烧时间、磁场强度等工艺参数对铁品位及回收率的影响规律。结果表明,在褐煤添加量为18%,焙烧温度800℃,焙烧时间50 min,磁场强度0.24 T的条件下,精选后的铁精矿TFe品位可达到59%,铁回收率可达到80%。With lignite as the reductant, a method of reduction roasting and magnetic separation was introduced to recover iron from gold-cyanide residue. The impact of lignite dosage, roasting temperature, roasting time, magnetic field strength and other relevant parameters on the iron grade and recovery of the concentrate was investigated. Results show that, an iron concentrate with a TFe grade of 59% and an iron recovery of 80% was obtained under the condition of lignite dosage of 18% , roasting temperature of 800℃, roasting time of 50 min and magnetic field strength of 0.24 T.

关 键 词:氰化尾渣 赤铁矿 磁选 还原焙烧 

分 类 号:TD92[矿业工程—选矿]

 