连铸中、低碳钢时结晶器振动和润滑的关系  

Relation between mold oscillation & lubrication when medium & low carbon steel casted

在线阅读下载全文

作  者:盛义平[1] 张兴中[1] 

机构地区:[1]东北重型机械学院

出  处:《连铸》1997年第2期8-11,共4页Continuous Casting

摘  要:在研究结晶器振动参数和保护渣耗量对低碳钢(C%<0.08)和中碳钢(0.07<C%<0.16)连铸坯振痕深度和对结晶器润滑的影响的基础上,提出了在浇铸低碳钢和中碳钢时,当连铸机在稳定浇铸过程中使负滑动时间t_N和保护渣耗量Q均取最佳值且在因工况变化短时间改变拉速时仍使t_N和Q的值始终在最佳值附近的f—V_c模型。A method for getting optimum oscillation amplitude and frequence has been proposed on the basis of researching the effect of the oscillation parameters and mold powder consumption on the oscillation mark depth of low carbon (C<0. 08%) and medium carbon (0. 07<C<0. 16%) steel slabs casted continuously. A new f-Vc pattern has also been proposed, which makes negative strip time tN and mold powder consumption Q get optimum value under steady running and be always near optimum value during understable running.

关 键 词:保护渣 结晶器振动 低碳钢 中碳钢 连铸机 最佳值 滑动时间 润滑效果 拉坯速度 拉速 

分 类 号:TF341.6[冶金工程—冶金机械及自动化]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象