机构地区:[1]青海大学机械工程学院,青海西宁810016 [2]黄河鑫业有限公司,青海西宁810008
出 处:《中国有色冶金》2011年第6期6-8,共3页China Nonferrous Metallurgy
摘 要:电解槽启动后期的工艺技术条件控制极为重要,主要目的是形成良好的炉帮,同时炉底不能形成大量结壳,以便电解槽平稳、高效生产和延长使用寿命。在实践中总结出了350 kA电解槽高温、高分子比、高电压、高电解质、低铝水平、低氧化铝浓度的"四高两低"启动后期管理工艺制度。The process technical conditions control of aluminum reduction cell in the later period of start up is very important, the purpose of this stage is to form good hearth and a few crusts formed at the bottom, so as to stable and efficient the production of aluminum reduction cell and to prolong its service life. The process management system of 350kA aluminum reduction cell in the later period of start up was summarized in practice, it called 'Four-high and Two-low' including high temperature, high molecular ratio, high voltage, high electrolyte, low aluminum level, and low alumina concentration.
关 键 词:铝电解 350 kA预焙槽 技术控制 启动后期管理
分 类 号:TF821[冶金工程—有色金属冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.28