TiO_2/HAP/MWCNT纳米复合薄膜修饰电极伏安法测定工业废水中邻苯二胺  被引量:4

Voltammetric Determination of o-Phenylenediamine in Industrial Wastewater by An Electrode Modified with Nanocomposite Film of TiO_2/Hydroxyapatite/MWCNT

在线阅读下载全文

作  者:李俊华[1,2] 邝代治[1,2] 冯泳兰[1,2] 刘梦琴[1,2] 

机构地区:[1]衡阳师范学院化学与材料科学系,衡阳421008 [2]衡阳师范学院功能金属有机材料湖南省普通高等学校重点实验室,衡阳421008

出  处:《分析化学》2011年第12期1864-1870,共7页Chinese Journal of Analytical Chemistry

基  金:湖南省教育厅创新平台开放基金(Nos.09K099;10K010);衡阳市科技局工业科技支撑计划项目(Nos.2009KG23;2009KG50)资助

摘  要:利用壳聚糖溶液分散纳米二氧化钛(TiO2),纳米羟基磷灰石(HAP)和多壁碳纳米管(MWCNT)制备了新型纳米复合薄膜修饰电极。基于此电极建立了一种无汞、高灵敏度测定痕量邻苯二胺(o-PDA)的方法。采用扫描电镜(SCE)、循环伏安(CV)和交流阻抗(EIS)等方法对修饰电极进行了表征;并研究了o-PDA在修饰电极上的电化学行为和动力学性质。结果表明,o-PDA在TiO2/HAP/MWCNT修饰电极上出现了灵敏的氧化峰(Epa=0.538V),说明纳米复合薄膜对o-PDA的氧化有较好的协同催化作用;氧化过程是一个2电子和2质子参与的不可逆过程,电极过程受到扩散步骤控制,其标准速率常数为1701 s-1;利用此氧化峰可以进行痕量o-PDA的检测,其峰电流与o-PDA浓度在5.0×10-5~1.0×10-3 mol/L范围内呈良好的线性关系,相关系数为0.9976,检出限可达1.0×10-5 mol/L;复合薄膜修饰电极稳定性较好,可用于工业废水中o-PDA的现场快速检测,加标回收率在98.6%~104.6%之间。A nanocomposite film modified electrode was successfully prepared by dispersing titanium dioxide nanoparticles(TiO2),hydroxyapatite nanofibers(HAP) and multi-wall carbon nanotube(MWCNT) into chitosan solution.Based on this modified electrode,a mercury-free and highly sensitive method for the determination of o-phenylenediamine(o-PDA) was established.The prepared electrode was characterized by scanning electron microscope(SEM),cyclic voltammetry(CV) and alternating current impedance(EIS),and the electrochemical behaviors and kinetic properties of o-PDA on the modified electrode were investigated.The experimental results showed that a sensitive oxidation peak of o-PDA appeared at TiO2/HAP/MWCNT modified electrode(Epa=0.538 V),which illuminated the nanocomposite film had a good synergistic catalytic effect on the oxidation of o-PDA.Further experiments showed that the oxidation process was an irreversible process containing a two-electron and two-proton reaction.This electrode process was controlled by the diffusion step,and the standard rate constant was 1701/s.Trace level of o-PDA can be determined with this oxidation peak.The peak currents were linearly dependent on the o-PDA concentrations in the range of 5.0×10-5-1.0×10-3 mol/L with correlation coefficient of 0.9976 and detection limit of 1.0 ×10-5 mol/L.This nanocomposite modified electrode had favorable stability and had been applied to the quick determination of o-PDAin industrial wastewater,and the recovery was from 98.6% to 104.6%.

关 键 词:纳米二氧化钛 纳米羟基磷灰石 碳纳米管 化学修饰电极 邻苯二胺 

分 类 号:O657.1[理学—分析化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象