Leaching of low grade zinc oxide ores in Ida^(2-)-H_2O system  被引量:6

Ida^(2-)-H_2O体系浸出低品位氧化锌矿(英文)

在线阅读下载全文

作  者:窦爱春[1] 杨天足[1] 杨际幸[1] 吴江华[1] 王安[1] 

机构地区:[1]中南大学冶金科学与工程学院,长沙410083

出  处:《Transactions of Nonferrous Metals Society of China》2011年第11期2548-2553,共6页中国有色金属学报(英文版)

基  金:Project (2007CB613604) supported by the National Basic Research Program of China

摘  要:Ida2--H2O system(iminodiacetate aqueous solution) was used to leach a low grade zinc oxide ore for Zn extraction.The effects of leaching time,liquid-solid ratio(L/S),total concentration of Ida2-([Ida2-]T),leaching temperature and pH on Zn leaching recovery and the dissolution of impurities such as Ca,Mg,Cu,Ni,Fe,Pb and Cd were investigated.Results show that Ca,Mg and Fe in ores were hardly dissolved in alkalescent iminodiacetate aqueous solution,while valuable metals such as Cu,Ni,Pb and Cd were partly dissolved into leaching liquor with Zn.The recovery of Zn reaches 76.6% when the ores were leached for 4 h at 70 ℃ by 0.9 mol/L iminodiacetate aqueous solution with pH of 8 and L/S of 5:1.采用Ida2--H2O体系(亚氨二乙酸盐水溶液)处理高碱性脉石型低品位氧化锌矿,考察浸出时间、液固比、配体总浓度、温度及pH值对矿物中主金属Zn及杂质元素Ca、Mg、Cu、Ni、Fe、Pb、Cd的溶出影响。结果表明:在弱碱性Ida2--H2O体系中,Ca、Mg、Fe不会被大量溶出,有价金属Cu、Ni、Pb、Cd可部分随主金属Zn溶出而进入浸出液;在浸出时间4h、液固比5:1、配体总浓度0.9mol/L、温度70℃、pH8的优化条件下,锌浸出率为76.6%。

关 键 词:Ida2- zinc oxide ore LEACHING 

分 类 号:TF813[冶金工程—有色金属冶金]

 