摘  要:制备了多壁碳纳米管-聚甲基红膜修饰电极,用循环伏安法和线性扫描伏安法研究了L-色氨酸在修饰电极上的电化学行为.结果表明:在pH=1.8的HCl-KCl底液中,L-色氨酸在修饰电极上出现一不可逆的氧化峰,氧化峰电流与其浓度在6.0×10-6-1.0×10-4mol/L范围内具有良好的线性关系:Ip(A)=-8.6484×10-8-0.2636c(mol/l),相关系数R=-0.9972,检出限为2.0×10-6 mol/L,测定L-色氨酸样品回收率为96.2%-101.3%.Poly Methyl red Film/Multiwalled Carbon Modified Electrode was made. And electrochemical behavior of L-Tryptophan was studied with Cyclic voltammetry and Linear sweep vohammetry. The results indicated that there was an irreversible Oxidation peak of L-Tryptophan in HCl - KCl with pH = 1.8. Good linearity was found between oxidation peak current and concentration of L-Tryptophan - 8. 6484 × 10^ -8 - 0. 2636c(mol/l) , relative coefficient L. Recovery of L-Tryptophan in human urine was 96.2% in range from 6.0 × 10^ -6 to 1.0 × 10 ^-4mol/L. Ip(A) = R was 0. 9972 ,and a detection limit was 2.0× 10^ -6 mol/ -101.3%.

关 键 词:多壁碳纳米管 甲基红 修饰电极 L-色氨酸 

分 类 号:O657.1[理学—分析化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象