改善挤出吹塑制件壁厚均匀性的几种方法  被引量:15

Several Methods of Improving the Homogenization of Extrusion Blow Molding Products Thickness

在线阅读下载全文

作  者:李道喜[1] 李能文[1] 明浩[1] 黄虹[1] 

机构地区:[1]重庆理工大学材料科学与工程学院,重庆400054

出  处:《精密成形工程》2012年第1期54-57,共4页Journal of Netshape Forming Engineering

摘  要:概述了近年来改善挤出吹塑中空制件壁厚不均匀的方法及其进展,包括新牌号的树脂,新的型胚壁厚控制技术及新的挤出吹塑成形工艺。型胚控制技术主要介绍了异型口模和可调机头;新成形工艺包括3D中空吹塑,真空吸塑与挤出吹塑相结合的技术,型坯温差法及高压低温挤出吹塑技术。Recent progressing methods of improving the wall thickness of extrusion blow molded parts, including new brands of resin, the new technology of controlling the thickness of parison and new extrusion blow molding technology were in troduced. The mentioned parison thickness control technology contained special shaped die and adjustable die. The listed new extrusion blow molding technology covered three-dimensional hollow blow molding, parison temperature difference method, combination of partial vacuum forming and blow molding, and high pressure low-temperature extrusion blow molding technology.

关 键 词:挤出吹塑 异型口模 可调机头 三维中空吹塑 局部抽真空 型坯温差法 

分 类 号:TQ320.66[化学工程—合成树脂塑料工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象