锌浸渣的浮选高硫产品中硫磺与闪锌矿的分离  被引量:3

Study on Separating Sulfur from Sphalerite in Leached Zinc Residue After Floatation

在线阅读下载全文

作  者:冯其明[1] 黄海威[1] 欧乐明[1] 

机构地区:[1]中南大学资源加工与生物工程学院

出  处:《金属矿山》2012年第3期149-151,共3页Metal Mine

基  金:教育部高等学校博士点基金项目(编号:20090162110053)

摘  要:针对广东某冶炼厂锌加压浸出渣浮选后的高硫产品,采用抑锌浮硫工艺,以硫化钠和OL-IID为抑制剂、六偏磷酸钠为分散剂进行硫磺与闪锌矿的浮选分离,经1次粗选、2次扫选、4次精浮,最终得到硫品位为92.23%、含锌2.45%的硫磺精矿,以及锌品位为12.97%、含硫73.10%的锌精矿。与现有工艺相比,锌与硫得到了有效的分离与回收。Based on a kind of high sulphur products pressure-leached from zinc by means of sulphur preferential floatation,with interaction of sodium sulfide and OL-IID, as the depressant, and hexametaphosphate, as the despersing agent, earriedout the floatation separation of sulfur from sphalerite. Through the process of single-stage roughing, two-stage scavenging and four-stage cleaning, and eventually, the sulfur and zinc concentration respectively contain 92. 23% of sulfur with 2.45% of zinc, and 73.10% of sulfur with 12. 97% of zinc ,The Zinc and sulfur get effective separation and recovery compared to current process,

关 键 词:浸出渣 抑锌浮硫 锌硫分离 

分 类 号:TD952[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象