机构地区:[1]宿迁学院三系,江苏宿迁223800
出 处:《稀有金属与硬质合金》2012年第2期29-32,共4页Rare Metals and Cemented Carbides
基 金:宿迁学院高级人才启动基金(SQCGJ2010002);江苏省大学生实践创新训练计划项目(2010SSJ02);宿迁市指导性科技计划项目(ZD2010010)
摘 要:以硝酸镍为镍源,浓氨水为沉淀剂,水热法合成了花瓣状β-Ni(OH)2球和β-Ni(OH)2纳米片,该合成方法简单易行。利用XRD和SEM分别对合成试样进行物相和形貌分析。研究结果表明:当pH值和反应时间均相同时,低温有利于合成花瓣状β-Ni(OH)2球,高温有利于合成β-Ni(OH)2纳米片。当反应时间为48.0h和pH值为9.0时,180℃下合成了花瓣状β-Ni(OH)2球;240℃下合成了β-Ni(OH)2纳米片。通过考察水热条件对产物形貌的影响,探讨了花瓣状β-Ni(OH)2球和β-Ni(OH)2纳米片的形成机制。β-Ni(OH)2 petal-shaped sphere and nanoplate were synthesized by hydrothermal method with strong ammonia as the precipitator and nickel nitrate as the nickel source.The above synthesis method is simple and easy to operate.The phase structure and morphology were analyzed using XRD and SEM.The results show that under the same pH value and reaction time,low temperature is good for the synthesis of β-Ni(OH)2 petal-shaped sphere,while high temperature is good for the synthesis of β-Ni(OH)2 nanoplate.β-Ni(OH)2 petal-shaped sphere and nanoplate are obtained at 180 ℃ and 240 ℃,respectively,both by reacting at pH 9.0 for 48.0 h.Based on the effects of hydrothermal synthesis conditions on morphology of the sample,the formation mechanism of β-Ni(OH)2 petal-shaped sphere and nanoplate is discussed.
关 键 词:花瓣状β-Ni(OH)2球 β-Ni(OH)2纳米片 硝酸镍 浓氨水 水热法
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:3.21.186.117