Mechanism of micro-waviness induced KH_2PO_4 crystal laser damage and the corresponding vibration source  被引量:1

Mechanism of micro-waviness induced KH_2PO_4 crystal laser damage and the corresponding vibration source

在线阅读下载全文

作  者:李明全 陈明君 安晨辉 周炼 程健 肖勇 姜伟 

机构地区:[1]Center for Precision Engineering,Harbin Institute of Technology [2]Chengdu Fine Optical Engineering Research Center

出  处:《Chinese Physics B》2012年第5期34-42,共9页中国物理B(英文版)

基  金:Project supported by the National Natural Science Foundation of China (Grant No. 50875066)

摘  要:The low laser induced damage threshold of the KH2PO4 crystal seriously restricts the output power of inertial confinement fusion.The micro-waviness on the KH2PO4 surface processed by single point diamond turning has a significant influence on the damage threshold.In this paper,the influence of micro-waviness on the damage threshold of the KH2PO4 crystal and the chief sources introducing the micro-waviness are analysed based on the combination of the Fourier modal theory and the power spectrum density method.Research results indicate that among the sub-wavinesses with different characteristic spatial frequencies there exists the most dangerous frequency which greatly reduces the damage threshold,although it may not occupy the largest proportion in the original surface.The experimental damage threshold is basically consistent with the theoretical calculation.For the processing parameters used,the leading frequency of micro-waviness which causes the damage threshold to decrease is between 350-1 μm-1 and 30-1 μm-1,especially between 90-1 μm-1 and 200-1 μm-1.Based on the classification study of the time frequencies of microwaviness,we find that the axial vibration of the spindle is the chief source introducing the micro-waviness,nearly all the leading frequencies are related to the practical spindle frequency(about 6.68 Hz,400 r/min) and a special middle frequency(between 1.029 Hz and 1.143 Hz).The low laser induced damage threshold of the KH2PO4 crystal seriously restricts the output power of inertial confinement fusion.The micro-waviness on the KH2PO4 surface processed by single point diamond turning has a significant influence on the damage threshold.In this paper,the influence of micro-waviness on the damage threshold of the KH2PO4 crystal and the chief sources introducing the micro-waviness are analysed based on the combination of the Fourier modal theory and the power spectrum density method.Research results indicate that among the sub-wavinesses with different characteristic spatial frequencies there exists the most dangerous frequency which greatly reduces the damage threshold,although it may not occupy the largest proportion in the original surface.The experimental damage threshold is basically consistent with the theoretical calculation.For the processing parameters used,the leading frequency of micro-waviness which causes the damage threshold to decrease is between 350-1 μm-1 and 30-1 μm-1,especially between 90-1 μm-1 and 200-1 μm-1.Based on the classification study of the time frequencies of microwaviness,we find that the axial vibration of the spindle is the chief source introducing the micro-waviness,nearly all the leading frequencies are related to the practical spindle frequency(about 6.68 Hz,400 r/min) and a special middle frequency(between 1.029 Hz and 1.143 Hz).

关 键 词:laser induced damage threshold micro-waviness Fourier modal theory power spectrum density 

分 类 号:O734[理学—晶体学] TN249[电子电信—物理电子学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象