工业Mo-Ni/USY-Al_2O_3失活催化剂的再生行为  被引量:5

Regeneration Behavior of Comercial Deactivated Mo-Ni/USY- Al_2O_3 Catalyst

在线阅读下载全文

作  者:孙万付[1] 马波 张喜文[2] 索继栓[1] 李树本[1] 罗锡辉[2] 

机构地区:[1]中国科学院兰州化学物理研究所OSSO国家重点实验室,兰州730000 [2]中国石油化工集团公司抚顺石油化工研究院,抚顺113001

出  处:《催化学报》2000年第2期156-160,共5页

摘  要:用ESCA ,XRD ,SEM及TPR等手段表征了不同条件下再生的工业失活加氢裂化催化剂 .结果表明 ,Mo Ni/USY Al2 O3 失活催化剂在实验室装置中快速再生优于慢速再生 ;再生温度对催化剂的结构与性能有影响 .480℃再生能将失活催化剂中绝大部分的碳和氮烧掉 ,且比表面积恢复率最高 ;6 0 0℃再生时 ,催化剂的毛细孔口明显减少 ,且产生少量聚结态 β NiMoO4Two regeneration methods (slow regeneration and fast regeneration) have been used to regenerate the industrial hydrocracking catalyst. It has been found that the fast regeneration method is better than the slow one for the deactivated Mo Ni/USY Al 2O 3 catalyst. The catalyst regenerated at different temperatures has been investigated by using TPR, XRD, SEM and XPS techniques. The results show that the recovery of surface area, relative crystallinity and mean pore size of the regenerated catalyst is over 90% comparing with the fresh one, when the regeneration temperature is 480 ℃. Considering other parameters, 480 ℃ has been chosen as the optimal regeneration temperature.

关 键 词:加氢裂子 分子筛 失活 再生 催化剂 

分 类 号:O643[理学—物理化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象