20G钢非金属夹杂物的行为研究  被引量:7

Research on non-metallic inclusions of 20G Steel

在线阅读下载全文

作  者:高菊[1] 李利杰[2] 

机构地区:[1]河北联合大学迁安学院,河北唐山063009 [2]河北钢铁集团宣化钢铁公司,河北宣化075100

出  处:《钢铁钒钛》2012年第3期93-97,共5页Iron Steel Vanadium Titanium

摘  要:针对某钢厂在生产20G钢初期,存在表面裂纹,低倍检验不合格的问题,对其生产过程中非金属夹杂物类型、数量、来源、尺寸及分布进行了综合分析。研究表明:正常铸坯中显微夹杂物平均总体积率0.149%,连浇坯中显微夹杂物平均总体积率为0.184%;正常坯中大型夹杂物平均含量为1.81 mg/kg,连浇坯中含量为3.31 mg/kg,其夹杂物主要来源于结晶器液面保护渣,其次中包覆盖剂和钢包渣卷入也是钢水污染的一个原因。In the early production of 20G in Steel,crack defects and macro examination unqualified.So the type,resource,amount and distribution of non-inclusions are systemically studied by the actual combination of laboratory and field research methods for the production process of 20G steel,The result shows: Volume ratio of micro-inclusion is 0.149%and 0.184% in normal and casting clab;The content of macro-inclusion in normal and casting clab is 1.81 mg/kg and 3.31 mg/kg.Inclusions are mainly derived from the mold surface with the flux,followed by Tundish complex agent and slag ladle complex.

关 键 词:20G钢 显微夹杂物 大型夹杂物 体积率 

分 类 号:TF762[冶金工程—钢铁冶金] TG115.21[金属学及工艺—物理冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象