检索规则说明:AND代表“并且”;OR代表“或者”;NOT代表“不包含”;(注意必须大写,运算符两边需空一格)
检 索 范 例 :范例一: (K=图书馆学 OR K=情报学) AND A=范并思 范例二:J=计算机应用与软件 AND (U=C++ OR U=Basic) NOT M=Visual
机构地区:[1]武汉大学化学系,武汉430072
出 处:《高等学校化学学报》2000年第5期694-697,共4页Chemical Journal of Chinese Universities
基 金:国家自然科学基金!(批准号:29870522);国家教委博士点基金
摘 要:以聚四氟乙烯(PTFE)悬浮体为氟化剂,悬浮体制样/氟化辅助电热蒸发(ETV)/ICP-AES直接测定TiO2陶瓷粉末中痕量杂质钇;考察了影响基体和待测元素的蒸发过程的各种因素;对比研究了待测元素和基体的氟化蒸发行为;实现了基体和待测元素的预分离,显著降低了基体效应.本法的检出限为0.26 μg/L,相对偏差为 3.8%(n=5, c=0. 5 mg/L).By using a polytetrafluorethylene(PTFE) emulsion as fluorinating reagent, a method for fluorinating assisted eletrothermal vaporization (ETV)/ICP-AES direct determination of trace yttrium in TiO2 ceramic powder has been proposed; the various facts which would affect the vaporization process between the matrix and the analyte were studied ; the fluorinating vaporization behavior of the matrix and the analyte both in slurry and in solution were investigated. Based on pre-separation between the matrix and the analyte, the matrix effect was reduced. On the optimum experiment conditions, the detection limit of the present method is 0.26μg/L; and the RSD is 3. 8 % (n=5, c=0.5 mg/L). This method has been applied to directly determinate trace yttrium in two kinds of TiO2 powder without any chemical pretreatment.
关 键 词:悬浮体制样 ICP-AES 痕量杂质 钇 二氧化钛陶瓷
分 类 号:TQ174.18[化学工程—陶瓷工业] O614.322[化学工程—硅酸盐工业]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.170