中厚板表面夹渣缺陷分析与研究  被引量:8

Analysis on Surface Slag Inclusion Defect of Medium and Heavy Plate

在线阅读下载全文

作  者:刘志勇[1] 孟根巴根[1] 王丽云[1] 臧淼[1] 尹绍江[1] 

机构地区:[1]唐山钢铁有限公司

出  处:《宽厚板》2012年第3期31-33,共3页Wide and Heavy Plate

摘  要:通过对夹渣缺陷处夹杂物的扫描电镜分析,铸坯皮下夹渣的产生原因是结晶器流场不合理,保护渣随结晶器内钢液流动卷入铸坯所致。通过改进浸入式水口形状、尺寸,优化浸入式水口插入深度,优化结晶器保护渣理化指标等工艺措施,可以有效减少连铸坯夹渣类缺陷。By means of scanning electron microscopy analysis on slag inclusion defect, it is found out that the slag inclusion at subsurface of the strand were caused by improper flow field inside the mould and mould powder was entrapped into strand by flowing liquid steel inside the mould. SLag inclusion type defects of continuous cast slab can be effectively controlled by technological measures such as improvement on the profile and size of submerged nozzle,opti- mization of immerged devth of submerged nozzle and physical and chemical indexes of the mould powder.

关 键 词:夹渣 流场 保护渣 

分 类 号:TF777[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象