提高3KG金锭物理合格率  被引量:1

Improving the Physical Passing Rate of 3KG Gold Bullion

在线阅读下载全文

作  者:董武斌[1] 夏彬[1] 邹震武[1] 

机构地区:[1]江西铜业集团公司贵溪冶炼厂,江西贵溪335424

出  处:《铜业工程》2012年第4期10-11,28,共3页Copper Engineering

摘  要:主要分析了传统立模模具浇铸口小,散热慢;微量杂质以及普通坩埚影响金锭物理合格率低的原因。介绍了把传统坩埚更换成高纯石墨坩埚,水冷双管平模模具。增加氧化除杂,液化气保温,盐酸漂洗工序措施。金锭物理合格率和直收率都达到提高,返炉率有所下降。This paper mainly analyzes the reason why that small caliber in vertical mould,slow heat dissipation,trace impurity,and crucible results in low physically qualified rate of the gold bullion.It introduces the traditional crucible was replaced by high purity graphite crucible,,the water cooled twin pipe flat mould,the increased oxidative removal of impurity,heat insulation by liquefied petroleum gas and hydrochloric acid rinsing process.Due to the measures,the gold bullion physically qualified rate and direct recovery rate increased,and the returned furnace rate declined.

关 键 词:平模 金锭 物理合格率 直收率 反炉率 

分 类 号:TF831[冶金工程—有色金属冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象