ICP-AES法测定锡精矿中锡、铜、铅、铁的含量  被引量:8

Determination of Sn,Cu,Pb and Fe in Tin Concentrate by Inductively Coupled Plasma Atomic Emission Spectrometry

在线阅读下载全文

作  者:李佗 杨军红 

机构地区:[1]西部金属材料股份有限公司理化检验中心,陕西宝鸡721014

出  处:《化学分析计量》2012年第6期73-75,共3页Chemical Analysis And Meterage

摘  要:建立了过氧化钠熔融分解样品、电感耦合等离子发射光谱法(ICP–AES)测定锡精矿中锡、铜、铅、铁的新方法。对试样分解方法、过氧化钠用量、元素分析谱线等进行了讨论。选择过氧化钠用量为2.0 g,样品熔融温度为850℃,锡、铜、铅、铁分析谱线分别为189.991,324.754,220.353,259.940 nm。将该方法应用于标准样品(BY0107–1)中Sn,Cu,Pb,Fe的测定,待测元素的回收率在92.0%~101.6%之间,检出限为分别为0.006,0.002,0.005,0.001μg/mL,测定结果的相对标准偏差为0.16%~2.11%(n=5)。A new method was established for the determination of Sn, Cu, Pb, Fe in tin concentrate by Inductively Coupled Plasma Atomic Emission Spectrometry(ICP-AES) with sodium peroxide melting. The way of sample decomposed, the amount of sodium peroxide and the analytical lines were discussed. 1.5 g Na2O2 and 850℃ were used in the sample decomposed. The analysis spectral lines of 189.991,324.754,220.353,259.940 nm were selected to measure Sn, Cu, Pb and Fe, respectively. The method was applied to determine Sn, Cu, Pb, Fe in standard samples(BY0107-1). The results were satisfactory with the RSD(n=5) in the range of 0.16%--2.11%, and the recoveries were 92.0%--101.6%, the detection limits were 0.006,0.002,0.005,0.001 ~g/mL, respectively.

关 键 词:ICP-AES 锡精矿     

分 类 号:O657.31[理学—分析化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象