Effect of galvanic contact on the flotability of galena in the presence and absence of a collector  被引量:2

Effect of galvanic contact on the flotability of galena in the presence and absence of a collector

在线阅读下载全文

作  者:M.B.Eslami Andargoli S.Jannesar Malakooti F.Doulati Ardejani H.Abdollahi 

机构地区:[1]Mining Engineering Department,Savadkooh Branch,Islamic Azad University,Savadkooh 447151333,Iran [2]Mineral Processing Engineering Department,Islamic Azad University,Langaroud Branch 447151333,Iran [3]Young Researchers Club,Islamic Azad University,Langaroud Branch 447151333,Iran [4]School of Mining,College of Engineering,University of Tehran,Tehran 1439957131,Iran

出  处:《International Journal of Mining Science and Technology》2012年第5期629-632,共4页矿业科学技术学报(英文版)

基  金:supported by the Islamic Azad University,Savadkooh Branch

摘  要:In this paper,the effect of various electrochemical environments in the galena flotation is investigated.The electrochemical environments consisted of a ball mill for grinding of galena ore and a Denver flotation cell for flotation of galena in the laboratory scale.In order to achieve the maximum recovery with sodium hyposulfite,the concentrations of 0.06 and 0.12 M of air and nitrogen gases have been used to control the pulp potential in the Denver flotation cell.The galena sample was from the ''Era mine'' which is located in the Kiyasar area,north of Iran.This mine contains:Galena(PbS) at least 22%,Fluorite(CaF 2) 73.37%,Quartz(SiO 2) 2.54% and other minerals such as Cerussite(PbCO 3) and Kaolinite(Al 2 Si 2 O 5(OH) 4).Flotation of Galena was conducted in a 0.12 M of sodium hyposulfite solution.It was found that the amount of recovery by this process was 85% and 63% in the presence and absence of potassium amyl xanthate(KAX) and at an estimated potential of 280 to 350 mV respectively while the recovery was 70% and 52% at an approximate potential of 175 to 210 mV in water in the presence and absence of collector(KAX).In this paper,the effect of various electrochemical environments in the galena flotation is investigated.The electrochemical environments consisted of a ball mill for grinding of galena ore and a Denver flotation cell for flotation of galena in the laboratory scale.In order to achieve the maximum recovery with sodium hyposulfite,the concentrations of 0.06 and 0.12 M of air and nitrogen gases have been used to control the pulp potential in the Denver flotation cell.The galena sample was from the ''Era mine'' which is located in the Kiyasar area,north of Iran.This mine contains:Galena(PbS) at least 22%,Fluorite(CaF 2) 73.37%,Quartz(SiO 2) 2.54% and other minerals such as Cerussite(PbCO 3) and Kaolinite(Al 2 Si 2 O 5(OH) 4).Flotation of Galena was conducted in a 0.12 M of sodium hyposulfite solution.It was found that the amount of recovery by this process was 85% and 63% in the presence and absence of potassium amyl xanthate(KAX) and at an estimated potential of 280 to 350 mV respectively while the recovery was 70% and 52% at an approximate potential of 175 to 210 mV in water in the presence and absence of collector(KAX).

关 键 词:Flotation Collector Galena Electrochemical Galvanic interactions 

分 类 号:TD951[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象