含硅氧化锌矿湿法冶金过程中脱镁试验研究  被引量:6

Experimental Study on Demagging in the Hydrometallurgical Process of Zinc Oxide Ore Bearing Silicon

在线阅读下载全文

作  者:马启坤[1] 

机构地区:[1]昆明冶金研究院,云南昆明650031

出  处:《云南冶金》2000年第3期22-25,共4页Yunnan Metallurgy

摘  要:试验证明了利用高硅氧化锌矿酸浸过程中所产生的可溶硅酸与硫酸镁反应生成硅酸镁沉淀的可能性。对影响脱镁反应参数的考察表明 ,镁的脱除率与可溶硅酸浓度及温度的高低密切相关 ,以其浓度表示则需大于 1 0g/LSiO2 ,脱镁温度 65℃左右为宜。Experimental results have confirmed the possibility of obtaining magnesium silicate by utilizing the soluble silicic acid,generated during the acid leaching of zinc oxide ore bearing high content of silicon,reacting with magnesium sulfate.The study on factors affecting the removal of magnesium indicated that the removal of magnesium was greatly influenced by the concentration of silicic acid and temperature.It has been explored that the condition with SiO 2 concentration of 10g/L and temperature of 65℃ is preferable.

关 键 词:含硅氧化锌矿酸浸 可溶硅酸 脱镁 湿法冶金 

分 类 号:TF813.032[冶金工程—有色金属冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象