海底管线钢X65生产工艺开发  被引量:3

Development of Technology for Producing X65 Submarine Pipeline Steel

在线阅读下载全文

作  者:王若钢[1] 刘浩岩[1] 应传涛[1] 王爽[2] 

机构地区:[1]鞍钢股份有限公司鲅鱼圈钢铁分公司,辽宁营口115007 [2]鞍钢股份有限公司技术中心,辽宁鞍山114009

出  处:《鞍钢技术》2013年第1期24-27,共4页Angang Technology

摘  要:对鞍钢鲅鱼圈5500 mm厚板生产线海底管线钢X65在不同季节的生产工艺进行了研究。不同季节条件下,精轧终轧温度和冷却后的返红温度对产品的屈强比及DWTT值影响明显。夏季采用较低的终轧温度及返红温度,抗拉强度提高;冬季提高终轧温度和返红温度,使DWTT值提高,韧性提升。采取相应的措施后,产品性能得到大幅提高。The technologies for producing X65 submarine pipeline steel by 5500 mm heavy plate production line in Bayuquan Iron Steel Subsidiary Company of Angang Steel Co.,Ltd.at different seasons are studied.Finishing temperatures and temperature rise after cooling have obvious influence on values of both yield ratio and DWTT of the steel.Tensile strength of the steel is increased with lower finishing temperature and temperature rise in summer while the DWTT value and toughness of the steel are increased with higher finishing temperature and temperature rise in winter.The properties of steel products are improved greatly after these corresponding countermeasures are taken.

关 键 词:海底管线钢 季节变化 生产工艺 力学性能 

分 类 号:TG335[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象