SPA-H集装箱板尾部翘皮检验与分析  被引量:1

Wrapping Inspection and Analysis of SPA-H Container Board Tail

在线阅读下载全文

作  者:赵景全 陈瑾 温寅 

机构地区:[1]山东日照钢铁集团有限公司,山东日照276806 [2]首钢迁钢集团,河北唐山063000

出  处:《物理测试》2013年第1期53-57,共5页Physics Examination and Testing

摘  要:对集装箱板在轧制过程中出现的翘皮问题进行电镜扫描及能谱分析,认为翘皮的产生是由于冶炼时保护渣未处理干净,同时由于加热或轧制时局部高温,产生氧化,在较浅的表面区域形成氧化物,当夹杂物较多且体积较大时,由于夹杂物距离表面较浅,经过多道次轧制后夹杂物从表面溢出,从而带动附近金属撕裂形成翘皮。The wrapping problem occurring in the rolling process was inspected by SEM(scanning electron microscope) and energy spectrum analysis.It is considered that wrapping is caused by unclean mould power in the process of iron-making.And because of part high temperature while heating and rolling,oxidation is generated and oxidation will be formed in the shallow surface area;when there is more inclusion and the volume is larger,because the distance from the surface of shallow inclusion is shallower,inclusion will overflow after multi-pass rolling and tear the near metal and wrapping is formed.

关 键 词:翘皮 夹杂物 带状组织 

分 类 号:TG335.5[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象