热拉伸对PGLA(90/10)纤维降解性能的影响  

Effect of hot drawing on the properties of PGLA (90/10) fiber during in vitro degradation

在线阅读下载全文

作  者:戴明欣[1] 梁超[1] 徐敏[1] 吴艳雪[1] 何雅琴[1] 张幼维[1] 赵炯心[1] 

机构地区:[1]东华大学纤维改性国家重点实验室,上海201620

出  处:《合成技术及应用》2013年第1期1-6,共6页Synthetic Technology & Application

摘  要:利用热拉伸获得不同性能与结构形态的PGLA(GA/LA摩尔比=90/10)纤维,并进行体外降解实验。在降解过程中,采用DSC、傅里叶红外光谱、扫描电镜等测试手段对PGLA(90/10)纤维的性能与形态变化进行研究。结果表明,热拉伸显著改变PGLA(90/10)纤维的降解特征。The PGLA (GA/LA molar ratio = 90/10) fibers with different properties and structural morphologies were obtained by heat-stretching treatment and were tested in vitro degradation. In the degradation process, the structures and properties of the PGLA(90/10) fiber have been investigated by means of DSC, infrared spectroscopy, scanning electron microscopy and other testing methods. The results show that, heat drawing can vary the degradation characteristics of the PGLA(90/10) fibers significantly.

关 键 词:PGLA(90 10)纤维 热拉伸 体外降解 

分 类 号:TQ342.2[化学工程—化纤工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象