纳米金/Nafion/石墨烯修饰玻碳电极检测对苯二酚的研究  被引量:11

Study on Determination of Hydroquinone Using Gold Nanoparticles/ Nafion/Graphene Modified Glassy Carbon Electrodes

在线阅读下载全文

作  者:孙雪[1] 康天放[1] 

机构地区:[1]北京工业大学环境与能源工程学院,北京100124

出  处:《分析测试学报》2013年第6期693-698,共6页Journal of Instrumental Analysis

基  金:北京市教委科技发展基金资助项目(KZ201110005006);北京市自然科学基金资助项目(8102009)

摘  要:采用一步电化学共还原的方法将纳米金(AuNPs)、Nafion、电化学还原石墨烯(ERGO)修饰到玻碳电极(GCE)表面,制成修饰电极AuNPs/Nafion/ERGO/GCE。以扫描电镜对其进行表征,用循环伏安法和微分脉冲伏安法研究对苯二酚在该修饰电极上的电催化行为。优化了实验参数,对苯二酚在2.0~100μmol/L及100~800μmol/L浓度范围内与其氧化峰电流呈良好的线性关系,检出限为0.3μmol/L。用该修饰电极成功地进行了实际水样中对苯二酚含量的测定。Au nanoparticles(AuNPs),Nafion and electrochemical reduced graphene oxide(ERGO) were modified onto the surface of a glassy carbon electrode(GCE) by one-step electrochemical co-reduction to fabricate a modified electrode of AuNPs/Nafion/ERGO/GCE.Scanning electron microscopy(SEM) was used to characterize the electrode.The electrocatalytical behaviors of the modified electrode towards hydroquinone(HQ) were investigated by cyclic voltammetry(CV) and differential pulse voltammetry(DPV).Experimental parameters were optimized.A good linear relationship between oxidation peak current of HQ and its concentration was obtained in the range of 2.0-100 μmol/L and 100-80 μmol/L ,with a detection limit of 0.3 μmol/L.This fabricated electrode was successfully applied in the determination of HQ in real samples.

关 键 词:电化学共还原 纳米金 石墨烯 对苯二酚 

分 类 号:O657.1[理学—分析化学] Q946.822[理学—化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象