作 者:盛敏奇[1,2] 钟庆东[2] 吕臣凯[1] 万康[1]
机构地区:[1]苏州大学沙钢钢铁学院,苏州215021 [2]上海大学上海市现代冶金与材料制备重点实验室,上海200072
出 处:《材料研究学报》2013年第3期267-272,共6页Chinese Journal of Materials Research
基 金:国家自然科学基金(51204115;50615024);新世纪优秀人才支持计划(NCET-07-0536)资助项目~~
摘 要:研究了超声波(100 W,100 kHz)对电沉积Co-Ni合金层的结构、形貌和性能的影响。结果表明:施加超声波可有效降低电沉积过程中浓差扩散的影响,促进阴极表面与镀液界面间的电子转移。超声波可降低Co-Ni合金层的Co含量并细化晶粒,使Co-Ni合金层更为平整。超声波影响Co-Ni合金层结构和形貌,可提高Co-Ni合金层的硬度以及在3.5%NaCl溶液中的耐腐蚀性。The effects of ultrasound agitation (100 W, 100 kHz) on the structure, morphology and prop- erties of electrodeposited Co-Ni alloy coatings were investigated in this paper. The result shows that: when ultrasonic agitation was used during the alloy coating electrodeposition, the concentration diffusion was effectively reduced, and the electron transfer between the cathode/solution interface was also pro- moted. Ultrasound agitation leads to the increase of Co content in alloy coating. The Co-Ni alloy coating deposited under ultrasound agitation is more fine-grained and uniform. The ultrasound agitation can lead to the enhancement of hardness and corrosion resistance properties of Co-Ni alloy coatings.
关 键 词:材料失效与保护 Co-Ni合金层 电沉积 静态 超声波 电化学
分 类 号:TB304[一般工业技术—材料科学与工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.113