光整冷轧IF带钢色差成因研究  被引量:2

CAUSE OF CHROMATIC ABERRATION ON SKIN ROLLED IF STRIP

在线阅读下载全文

作  者:穆天啸[1] 王兴东[1] 彭炜[2] 李金[2] 陈晓文[2] 

机构地区:[1]武汉科技大学冶金装备及其控制教育部重点实验室,湖北武汉430081 [2]武汉钢铁股份有限公司冷轧总厂,湖北武汉430083

出  处:《上海金属》2013年第4期32-34,共3页Shanghai Metals

基  金:国家自然科学基金(51174151);湖北省科技厅自然科学基金重点项目(2010CDA023)

摘  要:某冷轧厂在光整过程中,在IF带钢表面两侧约100 mm范围内出现色差。通过有限元分析软件MSC.Marc建立了光整的三维动态有限元模型,并对工作辊施加弯辊力。对光整过程进行动态仿真研究,分析了IF带钢表面轧制应力分布与摩擦因数之间的关系,最终找出了色差产生的原因,并提出了改进措施。Chromatic aberration appeared about 100 mm width on both side surfaces of IF strip during skin roiling in a cold rolling factory. A three dimensional dynamic finite element model of the skin rolling process was established by means of MSC. Marc software, and the roll bending force was applied to the working roll. Subsequently, the dynamic emulation on the skin rolling process was performed, and the effect of friction coefficient on roiling stress distribution at the IF strip surface was analyzed. Finally, causes of the chromatic aberration generation were discovered, and the corresponding precautions were put forward.

关 键 词:冷轧光整机IF带钢 色差 有限元模型 

分 类 号:TG338[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象