作 者:孙海杰[1,2] 李帅辉[1] 田翔宇[3] 张元馨[1] 江厚兵[1] 刘寿长[1] 刘仲毅[1]
机构地区:[1]郑州大学化学与分子工程学院,河南郑州450001 [2]郑州师范学院化学系环境与催化工程研究所,河南郑州450044 [3]郑州大学基础医学院,河南郑州450001
出 处:《分子催化》2013年第4期362-370,共9页Journal of Molecular Catalysis(China)
基 金:国家自然科学基金(21273205);国家科技型中小企业创新基金(10C26214104505);中国博士后科学基金(2012M511125);郑州大学优秀博士论文培育基金
摘 要:共沉淀法制备了Ru-Fe(x)催化剂,并利用X射线衍射(XRD)、X射线荧光光谱(XRF)、N2物理吸附和透射电镜等手段对催化剂进行了表征.结果表明,Ru-Fe(x)催化剂中助剂Fe以Fe3O4形式存在.单独Fe3O4并不能提高Ru催化剂的环己烯选择性.但在加氢过程中Fe3O4可与反应修饰剂ZnSO4反应生成(Zn(OH)2)3(ZnSO4)(H2O)x(x=1 or 3).化学吸附的(Zn(OH)2)3(ZnSO4)(H2O)x(x=1 or 3)在提高Ru催化剂环己烯选择性中起着关键作用.此外,Ru-Fe(x)催化剂的性能还与浆液中的Zn2+浓度和pH值有关.在0.61 mol/L ZnSO4溶液中Ru-Fe(0.47)催化剂不但给出了56.7%的环己烯收率,而且具有良好的稳定性和重复使用性能.化学吸附在Ru表面的Fe2+同样能提高Ru催化剂的环己烯选择性.在0.29 mol/L和0.61 mol/L FeSO4溶液中Ru-Fe(0.47)催化剂上化学吸附Fe2+量近似,性能近似.因为Fe2+和Zn2+性质的差异,在0.29 mol/L和0.61 mol/L FeSO4溶液中Ru-Fe(0.47)催化剂的环己烯选择性分别低于在同浓度的ZnSO4溶液中的.The Ru-Fe (x) catalysts were prepared by a co-precipitation method. The catalysts were characterized by X-ray diffraction (XRD), X-fluorescence (XRF), N2 physisorption and transimission electron microscopy (TEM). The results showed that the promoter Fe existed as Fe304 in the catalysts. The Fe304 alone could not im- prove the selectivity to cyclohexene of Ru catalyst. However, the Fe3 O4 on the surface could react with the reaction modifier ZnSO4 to form the (Zn(OH)2)3(ZnSO4) (HzO)x(X= 1 or 3) salt. The chemisorbed (Zn(OH)2)3 (ZnSQ) (H2 O)x(X = 1 or 3 ) salt played a key role in improving the selectivity to cyclohexene. Besides, the per- formance of the Ru-Fe (0.47) catalyst was closely related to the concentration of Zn2~ and the pH values of the slur- ry. The Ru-Fe(0.47) catalyst not only gave a cyclohexene yield of 56.7% in the presence of 0.61 mol/L ZnSO4 , but has a good stability and an excellent reusability. The reaction modifier FeSO4 also could enhance the selectivity to cyclohexene of the Ru-Fe(0.47) catalyst since the chemisorbed Fez+ could not be reduce to the metallic Fe on Ru surface. The Ru-Fe(0.47 ) catalyst exhibited the similar performance in 0.29 mol/L and 0.61 mot/L of FeSO4 solutions due to the similar amounts of the chemisorbed Fe〉. The Ru-Fe (0.47) catalyst showed the lower selectiv- ity to cyclohexene in 0.29 moL/L and 0.61 mol/L of MnSO4 solutions than that in the same concentrations of ZnSQ for the different natures of Fe2+ and Zn2+.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:3.14.67.90