退火过程对高温Sm_2Co_(17)磁体性能的影响  被引量:2

Influence of Annealling Process on the High Temperature Magnetic Property of Sm_2Co_(17)

在线阅读下载全文

作  者:夏满龙[1] 孙威[1] 方以坤[1] 潘伟[1] 朱明刚[1] 李卫[1] 

机构地区:[1]钢铁研究总院功能材料研究所,北京100081

出  处:《金属功能材料》2013年第4期21-24,共4页Metallic Functional Materials

摘  要:对Sm(CobalFe0.07Cu0.088Zr0.025)7.6烧结磁体在不同回火工艺下的室温和高温磁学性质进行了系统研究。结果表明,不同的等温时效温度回火时,磁体剩余磁通密度Br和最大磁能积(BH)max的在室温下不会有太大变化。然而,在高温(500℃)情形下却有很大区别,在790~810℃,获得了最高的(BH)max和矫顽力。所以回火工艺对磁体的高温性能产生了很大影响。通过调整回火工艺,所得到的样品在500℃性能可以达到Hci=5.48kOe,(BH)max=12.45MGOe。The dependence of magnetic properties of Sm (COba1 Fe0.07 Cuo.o88 Zr0.025)7.6 sintered magnets on the aging process was systematically studied. With different isothermal aging temperature, the remanences Br and the maxi- mum energy products (BH)max at room temperature doesn't change much. However, it make a big difference in high temperature(500 ℃). The highest (BH)~x was acquired in 790-810 ℃. By adjusting the aging process, the properties of sample were Hd=5.48 kOe, (BH)max=12.45 MGOe in 500 ℃.

关 键 词:高温 SM2CO17 回火 矫顽力 

分 类 号:TM273[一般工业技术—材料科学与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象