陕南某钾钠长石矿选矿除铁试验研究  被引量:4

Experimental Study on Separation of Iron from Feldspar in Southern Shaanxi

在线阅读下载全文

作  者:柳溪[1] 高惠民[1] 岑对对[1] 姚建云[1] 罗国清[1] 

机构地区:[1]武汉理工大学资源与环境工程学院,湖北武汉430070

出  处:《非金属矿》2013年第5期43-45,共3页Non-Metallic Mines

摘  要:通过对陕南某长石矿进行选矿试验研究,确定了使用铁球介质磨矿,沉降法脱泥的工艺方案。采用磁选-脱泥-浮选的工艺流程,可由含Fe2O3为0.36%的原矿获得产率为76.9%、Fe2O3含量为0.04%的粗粒级长石精矿及产率为9.82%、Fe2O3含量为0.51%的细粒长石精矿。精矿总产率达86.72%。Through the experiments on the feldspar ore in Southern Shaanxi, the best process program is obtained using ball-milling techniques and sedimentation desliming. With the technological process of "magnetic separation- desliming- flotation, can obtain the coarse-grained feldspar concentrates with 0.04% FeaO3 content and a recovery rate of 76.9%, alongwith the fine-grained feldspar concentrates with 0.51% Fe2O3 content and a recovery rate of 9.82% from the crude ore with 0.36% Fe2O3 content. The concentrate total recovery rate is 86.72%.

关 键 词:长石 除铁 磨矿介质 脱泥 

分 类 号:TD973.5[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象