红麻全杆化机浆的制备  

Preparation of corrugated paper with full staff kenaf chemi-mechanical pulp

在线阅读下载全文

作  者:周晓强[1] 牛梅红[1] 李娜[1] 孙衍宁[1] 

机构地区:[1]大连工业大学轻工与化学工程学院,辽宁大连116034

出  处:《大连工业大学学报》2013年第4期252-254,共3页Journal of Dalian Polytechnic University

基  金:辽宁省教育厅创新团队项目(LS2010011)

摘  要:用红麻制取化学浆可生产中高档纸或纸板,但化学浆得率低,并且废液需要处理。对红麻全秆化学机械浆进行了研究,以提高红麻原料的利用率,减少废液污染负荷。采用NaOH作为红麻生产化机浆的化学处理剂,通过正交试验确定了红麻全杆NaOH化学机械浆制浆的适宜条件:温度80℃,处理时间40min,NaOH用量8%。经过机械处理后成浆的得率为84%,紧度为0.609g/cm3,撕裂指数为13.84mN.m2/g,环压指数为0.13N.m/g,打浆度为42°SR,耐折度为253.5次,成浆可以抄造瓦楞原纸。The intermediate-high rail paper and paper but the yield is low and the waste liquid must be board can be produced by kenaf chemical pulp, treated. So the chemical-mechanical pulping is adopted to produce corrugated paper to improve the utilization ratio and decrease contaminate pressure. With a series of orthogonal experiment, the condition for kenaf NaOH chemi-mechanical pulp are confirmed that the temperature is 80 ~C, medicine cook time The tightness 0. 609 g/cm^3, tearability is 13.84 mN· m^2/g, ring-sh beating degree is 42°SR, the yield is 84%, folding endurance is 253 sheet attained in this excellent condition are ideal. is 40 min, NaOH charge is 8%. aped pressure is 0.13 N · m/g, 5 degrees and the properties of sheet attained in this excellent condition are ideal.

关 键 词:红麻 化机浆 瓦楞原纸 

分 类 号:TS743[轻工技术与工程—制浆造纸工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象