天然低品位氧化锰矿生产活性二氧化锰  

Preparation of MnO_2 with low-grade NMD

在线阅读下载全文

作  者:张清岑[1] 袁明亮[1] 李贵奇 

机构地区:[1]中南工业大学矿物工程系,湖南长沙410083

出  处:《中南工业大学学报》2000年第2期117-120,共4页Journal of Central South University of Technology(Natural Science)

摘  要:为了改变优质电池原料短缺的状况和充分利用低品位锰矿资源 ,研究了天然低品位二氧化锰矿在添加少量无污染添加剂的条件下 ,在 71 0℃下焙烧 2h ,可使矿石中MnO2 转化为Mn2 O3 .其转化率达 99 5 %以上 .同时对焙烧产物进行岐化反应所用的酸介质、酸用量和反应时间与歧化作用的关系进行了研究 .并对氯酸钠氧化歧化液中Mn2 + 的氧化效果进行了分析 ,提出了分步氧化歧化液中Mn2 + 的新工艺 .MnO 2 can be converted into Mn 2O 3 with roasting time of 2 h at 710 ℃ by adding pollution free additive to low grade natural manganese dioxide ore and the efficiency is over 99.5%. The effects of acid type, the amount of acid and the reaction time on the disproportion process of the roasting product of NMD in acid solution are studied and a new process of fractional oxidation crystallization is suggested based on the study of the effect of acid amount and NaClO 3 on the oxidation of Mn 2+ in the disproportion solution. [

关 键 词:歧化 活性二氧化锰 氧化锰矿 添加剂 电池原料 

分 类 号:TD981[矿业工程—选矿] TM911.1[电气工程—电力电子与电力传动]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象