作 者:廖小丽[1] 肖连生[1] 孙亚辉[1] 曾理[1]
出 处:《有色金属(冶炼部分)》2014年第1期40-44,53,共6页Nonferrous Metals(Extractive Metallurgy)
基 金:国家高技术研究发展计划(863计划)项目(2007AA06Z129)
摘 要:采用新型萃取剂HBL101从镍钼矿焙烧料高酸浸出液中直接萃取钼。考察有机相组成、料液酸度、相比、振荡频率、平衡时间、温度对钼萃取过程的影响,并绘制了HBL101萃钼等温曲线。结果表明,在优化的工艺条件下,钼萃取率达96.8%以上,有机相饱和容量为12.09g/L;负载有机相用纯水洗涤后经3级逆流氨水反萃,钼反萃率达99.9%以上,实现了钼镍分离及钼的富集转型。A novel extractant of HBL101 was used to extract molybdenum directly from a strong acid leaching solution of Ni-Mo ore after roasting. The effects of organic phase composition, acidity of feed solution, phase ratio, oscillation frequency, equilibrium time and temperature on molybdenum extraction were investigated. The extraction isotherm of molybdenum with HBL101 was drawn. The results show that molybdenum extraction rate can reach 96.8% above and saturation capacity of organic phase is 12.09 g/L under the optimum conditions. The molybdenum back extraction rate is 99.9% above after the loaded organic phase is washed by pure water and three-stage of counter-current stripped by ammonia. Separation of molybdenum and nickel, as well as enrichment and transformation of molybdenum are finally achieved.
分 类 号:TF841.2[冶金工程—有色金属冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.117