高分散性芳纶短纤维TWAROND3500在矿山轮胎胎侧胶中的应用  被引量:4

Application of Aramid Fiber TWARON D3500 with Enhanced Dispersion Characteristics in the Sidewall Compound of Mining Tire

在线阅读下载全文

作  者:徐世传[1,2] 方永清[1,2] 

机构地区:[1]杭州中策橡胶有限公司新安江分公司,浙江新安江311607 [2]中策橡胶建德有限公司,浙江建德311607

出  处:《橡胶科技》2014年第1期31-33,共3页Rubber Science and Technology

摘  要:研究高分散性芳纶短纤维TWAROND3500在矿山轮胎胎侧胶中的应用。结果表明:在矿山轮胎胎侧胶中添加高分散性芳纶短纤维TWAROND3500可以明显降低胶料生热并提高耐磨性能,有利于延长轮胎使用寿命;高分散性芳纶短纤维TWAROND3500胎侧胶挤出和成型工艺性能好;高分散性芳纶短纤维TWAROND3500在胎侧胶中的适合用量为2~3份。In this study, aramid fiber TWARON D3500 with enhanced dispersion characteristics was applied in the sidewall compound of mining tire. The experimental results showed that the heat build-up of the vulcanizates was reduced and the abrasion resistance increased, indicating improved tire service life. TWARON D3500 offered enhanced dispersion characteristics, so that the processing properties of the sidewall compound were good during extrusion and molding processes. The optimum addition level of TWARON D3500 was 2-3 phr.

关 键 词:矿山轮胎 胎侧胶 高分散性芳纶短纤维 生热 耐磨性能 

分 类 号:TQ336.1[化学工程—橡胶工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象