保温时间对赤泥粉煤灰轻质保温砖性能的影响  

Influence of soaking time in firing on the properties of lightweight insulating red mud fly ash brick

在线阅读下载全文

作  者:马龙[1] 苏登成[2] 李国忠[1] 

机构地区:[1]济南大学材料科学与工程学院,山东济南250022 [2]苏州中材建设有限公司,江苏昆山215300

出  处:《砖瓦》2014年第4期12-14,共3页Brick-tile

摘  要:以赤泥、粉煤灰、膨润土为主要原料,掺加一定量的成孔剂和助溶剂,通过烧结制成赤泥轻质保温砖。利用扫描电子显微镜对赤泥轻质保温砖破坏断口进行了微观形貌分析,结果表明,在烧结温度为1100℃保温180 min,制得的保温砖性能较好,继续延长保温时间,保温砖试样性能基本不变。The lightweight insulation red mud brick is prepared by red mud, fly ash, bentonite as the main raw material, and some pore forming agent and fluxing agent. The influence of soaking time in firing on the properties of insulation red mud brick is studied. The fracture surface's microstructure of lightweight insulation brick is analyzed by scanning electron microscope (SEM) and the firing mechanism is discussed preliminarily. The results show that when firing temperature is 1100 ℃ and soaking time is 180 minutes, the thermal insulation of brick is better. While prolongs the soaking time, the performance of sample is almost invariable.

关 键 词:赤泥 轻质保温砖 保温时间 

分 类 号:TU522.01[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象