Synthesis, Characterization and Application of Methyl 3,5-Disulfo-benzoate Dipotassium Dihydrate as Nucleating Agent for Poly(L-lactide)  被引量:1

Synthesis, Characterization and Application of Methyl 3,5-Disulfo-benzoate Dipotassium Dihydrate as Nucleating Agent for Poly(L-lactide)

在线阅读下载全文

作  者:SUN Zhiqiang ZHANG Han PANG Xuan BIAN Xinchao CHEN Wenqi CHEN Xuesi 

机构地区:[1]Key Laboratory of Polymer Ecomaterials, Changchun Institute of Applied Chemistry,Chinese Academy of Sciences, Changchun 130022, P.R.China

出  处:《Chemical Research in Chinese Universities》2014年第2期333-338,共6页高等学校化学研究(英文版)

基  金:Supported by the National Natural Science Foundation of China(Nos.51203155,51173183,21004061,51021003) and the National High Technology Recearch Development Program of China(No.2011AA02A202).

摘  要:A newly synthesized aromatic sulfonate compound,complex 2 with formula of K2[H3COOC-C6H3(SO3)2]·2H2O(methyl 3,5-disulfo-benzoate dipotassium dihydrate) was synthesized and characterized by elemental analysis,infrared(IR) spectrometry,nuclear magnetic resonance(NMR) and crystal structure measurement.Single-crystal X-ray diffraction(XRD) revealed that complex 2 crystallized in the triclinic system with space group P(i).Complex 2 was used as nucleating agent for poly(L-lactide)(PLLA).The crystallization of PLLA with powder of complex 2 was investigated by means of differential scanning calorimetry(DSC) and polarized optical microscopy (POM).The results prove that complex 2 was effective as nucleating agent for PLLA.It could accelerate crystallization by reducing the induction time and increasing the density of nuclei in the crystallization process.The half-time of crystallization(t0.5) for pure PLLA was about 8 times longer than that of PLLA sample with 1.0%(mass fraction) of complex 2.A newly synthesized aromatic sulfonate compound,complex 2 with formula of K2[H3COOC-C6H3(SO3)2]·2H2O(methyl 3,5-disulfo-benzoate dipotassium dihydrate) was synthesized and characterized by elemental analysis,infrared(IR) spectrometry,nuclear magnetic resonance(NMR) and crystal structure measurement.Single-crystal X-ray diffraction(XRD) revealed that complex 2 crystallized in the triclinic system with space group P(i).Complex 2 was used as nucleating agent for poly(L-lactide)(PLLA).The crystallization of PLLA with powder of complex 2 was investigated by means of differential scanning calorimetry(DSC) and polarized optical microscopy (POM).The results prove that complex 2 was effective as nucleating agent for PLLA.It could accelerate crystallization by reducing the induction time and increasing the density of nuclei in the crystallization process.The half-time of crystallization(t0.5) for pure PLLA was about 8 times longer than that of PLLA sample with 1.0%(mass fraction) of complex 2.

关 键 词:Nucleating agent Crystal structure Poly(L-lactide) Isothermal crystallization 

分 类 号:TQ325.14[化学工程—合成树脂塑料工业] O614.33[理学—无机化学]

 