Investigation on the relationship between hearth wall erosion and deadman permeability for large blast furnaces  被引量:1

Investigation on the relationship between hearth wall erosion and deadman permeability for large blast furnaces

在线阅读下载全文

作  者:XU Wanren MAO Xiaoming ZHU Jinming LIU Kaihua 

机构地区:[1]Research Institute,Baoshan Iron & Steel Co.,Ltd [2]Ironmaking Plant,Baoshan Iron & Steel Co.,Ltd

出  处:《Baosteel Technical Research》2014年第2期1-11,共11页宝钢技术研究(英文版)

摘  要:In this study, the relationship between hearth wall erosion and deadman permeability was investigated based on the change in the hearth bottom and hearth sidewall temperatures. Additionally, the operation practice for controlling hearth wall erosion in the large No. 1 blast furnace at Baosteel was also investigated. The reasons for the decrease in the permeability of deadman coke were analyzed, and measures for improving the permeability of deadman coke and controlling hearth wall temperature rising were described. The results show that a decrease in deadman coke permeability is the main reason for refractory temperature increase and hearth wall erosion. This indicates the importance of monitoring changes in hearth working conditions and taking appropriate measures to maintain sufficient permeability of the deadman and balance the hot metal flow and drainage of slag. At this rate, the decline in the hearth bottom temperature and fast rising of the hearth wall temperature can be restrained.In this study, the relationship between hearth wall erosion and deadman permeability was investigated based on the change in the hearth bottom and hearth sidewall temperatures. Additionally, the operation practice for controlling hearth wall erosion in the large No. 1 blast furnace at Baosteel was also investigated. The reasons for the decrease in the permeability of deadman coke were analyzed, and measures for improving the permeability of deadman coke and controlling hearth wall temperature rising were described. The results show that a decrease in deadman coke permeability is the main reason for refractory temperature increase and hearth wall erosion. This indicates the importance of monitoring changes in hearth working conditions and taking appropriate measures to maintain sufficient permeability of the deadman and balance the hot metal flow and drainage of slag. At this rate, the decline in the hearth bottom temperature and fast rising of the hearth wall temperature can be restrained.

关 键 词:large blast furnace HEARTH DEADMAN PERMEABILITY hearth wall refractory erosion 

分 类 号:TF549[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象