熔融还原合成渣中碳还原Fe_2O_3的发泡特性参数  被引量:3

Foam Behavior Parameters for Foaming Caused by Reducing Fe_2O_3 with Graphite in the Synthetic Slag of Smelting Reduction

在线阅读下载全文

作  者:吴铿[1] 张二华[1] 储少军[1] 陈春元[1] 李洪民[1] 郭映波[1] 

机构地区:[1]北京科技大学冶金学院,北京100083

出  处:《北京科技大学学报》2001年第3期204-207,共4页Journal of University of Science and Technology Beijing

基  金:国家自然科学基金资助项目(No.59974002)

摘  要:测定了Fe2O3在熔融还原合成渣中被碳还原时,还原气体产生泡沫渣的高度与时间的 关系.由发泡特性参数方程计算了不同条件下的发泡特性参数,从而可以对熔融还原过程中由 内生气源引起的发泡过程进行定量描述。为在铁浴中控制泡沫渣现象提供了必要的基础.The relationship between the foam height and time has been measured for foaming processes caused by reducing Fe2O3 in smelting reduction synthetic slap. The foam behavior parameters under different condition were determined by means of experimental results and foam behavior equations. In this way, the fo- aming process caused by reducing Fe2O3 in smelting reduction process could be described quantitatively. The results provide necessary basis for controlling the foam phenomenon in iron bath.

关 键 词:泡沫渣 内生气源 熔融还原 发泡特性参数 氧化铁 发泡过程 泡沫化指数 

分 类 号:TF533.1[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象