燃料电池用碱性阴离子交换膜链结构调控研究进展  被引量:5

Progress of polymer chain structure regulation of alkaline anion-exchange membranes for fuel cells

在线阅读下载全文

作  者:司江菊 卢善富 相艳 Jiangju Si;Shanfu Lu;Yan Xiang(Beijing Key Laboratory of Bio-inspired Energy Materials and Devices,School of Space and Environment,Beihang University,Beijing 100191,China;School of Chemistry and Chemical Engineering,Xinxiang University,Xinxiang 453003,China)

机构地区:[1]北京航空航天大学空间与环境学院仿生能源材料与器件北京市重点实验室,北京100191 [2]新乡学院化学化工学院,新乡453003

出  处:《科学通报》2019年第2期153-164,共12页Chinese Science Bulletin

基  金:国家自然科学基金(21722601;21576007);北京市重点研发计划(Z171100000917011)资助

摘  要:碱性阴离子交换膜燃料电池(AAEMFCs)因氧还原动力学快、可使用非Pt催化剂、成本低等优点迅速发展成燃料电池的重点研究领域.作为AAEMFCs的核心组件,碱性阴离子交换膜(AAEMs)的性能直接影响着燃料电池的输出性能和使用寿命.为保证燃料电池高效、稳定、长时间的运行,AAEMs应具备高的离子电导率、尺寸及化学稳定性.但目前开发的膜尚难同时满足这些要求,在实际应用中依然面临阴离子传输效率与尺寸稳定性难以兼顾、碱性稳定性较差等问题.本文将结合近年来国内外及本课题组的研究进展,梳理AAEMs发展中存在的关键问题与解决思路,展望未来的发展方向.Alkaline anion-exchange membrane fuel cells(AAEMFCs) have attracted worldwide interest due to their advantages including fast oxygen reduction kinetics, high compatibility with non-precious-metal catalyst and low cost. As one of the key components in AAEMFCs, the performance of alkaline anion exchange membranes(AAEMs) directly affects the power output and durability of the fuel cells. During fuel cell operating, AAEMs require high ionic conductivity, excellent dimensional and chemical stability to ensure high efficiency and outstanding durability. However, it is still difficult for any type of the AAEMs to meet all these requirements. This monograph summarizes recent development around the world for AAEMs, especially for the trade-off effect between ionic conductivity and stability of AAEMs as well as the proposed strategies for this issue. The charge carrier in AAEMs is OH^-, and it has a lower transporting efficiency owing to its lower mobility, higher dependence on water molecular and the blocking of many hydrophobic domains in AAEMs. The improvement of ion-exchange capacity(IEC) by increasing the grafting degree(GD) of cationic functional groups can, to some extent, solve this issue. however, a high GD always bring the following negative issues:(1) Excessive swelling of AAEMs and significant reducing in the dimensional stability of membranes;(2) the increase of OH^-concentration accelerates the kinetics of nucleophilic substitution and Hofmann elimination, leading to the degradation of cationic groups;(3) the enhanced polarization of the cationic groups and the hydrophilicity of the main chain enable the polymer backbone susceptible to nucleophilic attack by OH^-, resulting in the degradation of the membrane, and even short-circuit of the fuel cells. In order to solve these issues, various of polymer chain architectures have been designed and regulated. To balance the ionic conductivity and the dimensional stability in AAEMs, double, triple and multi-cations are grafted on one site of polymer backbone to achi

关 键 词:燃料电池 碱性阴离子交换膜 离子电导率 碱性稳定性 微观结构 

分 类 号:TM911.4[电气工程—电力电子与电力传动]

 