机构地区:[1]抚顺石油化工研究院九室 [2]抚顺石油学院应用化学系,辽宁省抚顺市113001
出 处:《光谱实验室》2002年第4期528-531,共4页Chinese Journal of Spectroscopy Laboratory
摘 要:用电感耦合等离子体发射光谱 (ICP- AES)法同时测定加氢裂化催化剂中 Fe、Ni、Cu、V、Pb的含量 ,以氢氟酸 -盐酸处理样品 ,优选了分析线和积分时间。此 5种被测元素回收率在 95 %— 10 5 %之间 ,相对标准偏差 <6 %,各元素的检出限依次为 :0 .0 0 0 5、0 .0 0 2、0 .0 14、0 .0 0 0 5、0 .0 0 2 9μg/ m L。The method of ICP-AES for simultaneous determination of iron, nickel, copper,vanadium and lead content in hydrocracking catalyst has been studied.Using hydrofluoric acid and hydrochloric acid to digest the samples,the analysis line and integration time were optimized.The relative standard deviation of the method is less than 6% and the recovery of Fe,Ni,Cu,V,Pb are within 95%-105%.The detection limit for these 5 elements are 0.0005,0.002,0.014,0.0005,0.0029μg/g respectively.This method is rapid,accurate and reliable.
关 键 词:ICP-AES法 同时测定 电感耦合等离子-原子发射光谱 加氢裂化催化剂 铁 镍 铜 钒 铅
分 类 号:TE624.9[石油与天然气工程—油气加工工程] TQ426.95[化学工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:3.133.141.1