催化加氢合成浅色度C_5石油树脂  被引量:2

Preparation of light-colored C_5 petroleum resin by catalytic hydrogenation

在线阅读下载全文

作  者:陆敏[1] 文艺[1] 李树白[1] 刘承先[1] 程进[1] 

机构地区:[1]常州工程职业技术学院化学工程技术系,江苏常州213164

出  处:《化工进展》2014年第9期2339-2343,共5页Chemical Industry and Engineering Progress

摘  要:通过对C5石油树脂的催化加氢,合成了浅色度C5石油树脂,制备并筛选了催化剂,采用固定床反应器对C5石油树脂进行了加氢工艺研究,采用BET、SEM和DTA-TG对催化剂进行了表征,用IR对C5石油树脂加氢前后的结构进行了分析。研究结果表明,Ni基多金属催化剂C5JH-3在原料浓度为20%、温度为220-240℃、压力3.5MPa、空速0.5h-1、氢油比600∶1的条件下对C5石油树脂加氢,可制得软化点高的浅色度树脂。To obtain light-colored C5 petroleum resin , C5 petroleum resin was catalytically hydrogenated in a fixed-bed hydrogenation micro reactor. The C5 petroleum resin hydrogenation process was studied. Several hydrogenation catalysts were prepared and compared. The catalysts were characterized by nitrogen adsorption-desorption (BET),scanning electron microscopy (SEM) and differential thermal analyzer (DTA-TG). The petroleum resin and hydrogenated petroleum resin were characterized by FT-IR spectroscopy. The high softening point and light-colored C5 petroleum resin was obtained under the condition of Ni multi-metal catalyst C5JH-3,raw resin concentration of 20%, temperature of 220-240℃,pressure of 3.5MPa,space velocity of 0.5h-1,and hydrogen to oil ratio of 600∶1.

关 键 词:C5石油树脂 催化剂 催化 加氢 

分 类 号:TQ322.4[化学工程—合成树脂塑料工业] TQ626.94

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象