机构地区:[1]西安工程大学纺织与材料学院,陕西西安710048
出 处:《西安工程大学学报》2014年第4期418-421,共4页Journal of Xi’an Polytechnic University
基 金:国家自然科学基金资助项目(50572084);陕西省自然科学基金资助项目(2012JQ6011);陕西省重点实验室专项资助项目(12JS044)
摘 要:以Ca(NO3)2·4H2O和P2O5为前驱体,无水乙醇为溶剂,采用Sol-Gel法制备HAP纳米材料.通过扫描电镜对HAP样品的颗粒形貌和粒度尺寸进行表征,并用X衍射分析仪对HAP样品进行物相分析.对比研究了水浴温度、陈化时间和焙烧温度等因素对HAP纳米材料性能的影响.得出制备纳米羟基磷灰石材料的最佳工艺条件:水浴温度40℃,陈化时间70h,焙烧温度800℃.Hydroxyapatite nano-materials were prepared through sol-gel ,reactant calcium nitrate (Ca (NO3 )2 · 4H2 O) and phosphorus pentoxide (P2 O5 ) are used as precursor and absolute alcohol are used as solvent .The powder size and morphology were characterized by SEM .The phase analysis was done by XRD .The effect of water bath temperature ,aging time and roast temperature on the property of hydroxyapatite nano-materials were studied .The optimal reaction conditions are as follows :water bath temperature is 40℃ ,aging time is 70h ,roast temperature is 800℃ .
分 类 号:TB34[一般工业技术—材料科学与工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.248