HEDP在废纸浆H_2O_2漂白过程中的应用  被引量:4

The Application of HEDP in Hydrogen Peroxide Bleaching of Mixed Waste Paper Pulp

在线阅读下载全文

作  者:张妍[1] 惠岚峰[1] 刘忠[1] 熊皇伟 

机构地区:[1]天津科技大学天津市制浆造纸重点实验室,天津300457

出  处:《中国造纸》2015年第2期33-38,共6页China Pulp & Paper

摘  要:以混合废纸浆为原料,研究了羟基乙叉二膦酸(HEDP)作为螯合剂在废纸浆H2O2漂白中的应用。结果表明,预处理段螯合剂的最佳使用条件为:HEDP用量0.15%,螯合温度60℃,螯合时间45 min。在本实验所获得的HEDP最佳工艺条件下,与EDTA螯合剂的对比实验发现,HEDP的螯合效果优于EDTA的螯合效果;后续漂白段在Na2SiO3用量为3.0%时,可使废纸浆的白度达到76.6%,返黄值降低为1.76%;在HEDP最佳预处理条件下,在后续H2O2漂白中添加一定量的EDTA可使Na2SiO3的用量降低而不影响纸浆白度和手抄片的返黄值。Mixed waste paper pulp was bleached by using hydrogen peroxide and with 1-hydroxy ethylidene-1, 1-diphosphonic acid(HEDP) as the chelator . The results showed that the optimum conditions of chelating stage was as follows: HEDP dosage 0. 15% on OD pulp, tem- perature 60℃, time 45 min, the HEDP's chelating efficiency was better than the EDTA under the conditions ; The pulp whiteness reached to 76. 6% ISO and the PC value decreased to 1.76% ; in subsequent hydrogen peroxide bleaching when sodium silicate dosage was 3.0% , adding a certain amount of EDTA could reduce the dosage of sodium silicate without affecting the whiteness and P. C value.

关 键 词:混合废纸浆 H2O2漂白 羟基乙叉二膦酸 螯合剂 NA2SIO3 

分 类 号:TS745[轻工技术与工程—制浆造纸工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象